How do I Vaccum Bag this Air Box ??


Author
Message
Eddie Walsh
E
Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)Supreme Being (734 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Hi I have been looking at this Air Box and trying to figure out how I can Vaccum Bag ??? to me looks impossible, so any help appreciated, Regards DM
Attachments
458 Air Box.jpg (1.2K views, 1.00 MB)
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Dinoman - 7/13/2018 3:20:07 PM
Steve Broad - 7/13/2018 11:44:38 AM
A bit like this.

Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DM

I don't think you need to do it on your part (because I think once you blank off the two tubes in your mould you'll actually have no open ends on your moulding) but if you're struggling to understand how to bag a 'tube' then just think of creating a bag like a torus (donut). Bagging tubes is common practice.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
                                 Trapped moulds, been there and got the relevant T-Shirt :-)
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
                                             Hi Steve, how can I tell if my fibreglass woven matt that has chemical binders ??, Regards DM
Dinoman - 8 Years Ago
     A bit like this.
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
                                                 Hi Thank, can you also tell me where I can download the data Sheets from as I tried the search box but it came back with nothing, Regards DM
Dinoman - 7 Years Ago
                                                     If you are talking about EC's component prepregs, click on the datasheet button on the details page.
Steve Broad - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
                 Hey eddie! Any updates on airbox?
Furkan Yahsi - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago