How do I Vaccum Bag this Air Box ??


Author
Message
Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Hi I have been looking at this Air Box and trying to figure out how I can Vaccum Bag ??? to me looks impossible, so any help appreciated, Regards DM
Attachments
458 Air Box.jpg (1.2K views, 1.00 MB)
Reply
Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
oekmont - 1/18/2019 12:57:49 PM
No, not really. You should definitely not work at these temperatures. Especially not with high temp resins.
First: they tent to be thicker, wich makes them paste like at low temperatures. This means it is much more likely to trap air inside corners and inside the resin itself.
Secondly: if you use high temp resin you will likely heat the mould up to higher temperatures. This will let the trapped air expand, and ruin your mould surface.
It was you, who wanted to vacuum the mould, because he was fearing he would need to repair it because of trapped air, right? Working at low temperatures  is the most reliable way to cause exactly that.

Hi, Thanks again for the advice, but I have started so now I will have to finish as best I can, that was why I asked if there was any way of thinning it down, so is there any way to thin it down, Regards DM

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
                                 Trapped moulds, been there and got the relevant T-Shirt :-)
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
                                             Hi Steve, how can I tell if my fibreglass woven matt that has chemical binders ??, Regards DM
Dinoman - 8 Years Ago
     A bit like this.
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
                                                 Hi Thank, can you also tell me where I can download the data Sheets from as I tried the search box but it came back with nothing, Regards DM
Dinoman - 7 Years Ago
                                                     If you are talking about EC's component prepregs, click on the datasheet button on the details page.
Steve Broad - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
                 Hey eddie! Any updates on airbox?
Furkan Yahsi - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago