Hi I have been looking at this Air Box and trying to figure out how I can Vaccum Bag ??? to me looks impossible, so any help appreciated, Regards DM
|
|
Group: Forum Members
Posts: 52,
Visits: 294
|
+x+xHi Matt, Thanks again,as you can imagine I have quite a bit of Chopped mat Strand which I have used for my Fibreglassin so can I still use this with your HT Gel and Resin, also my MEKcat is that compatible, as I do not want to mix the wrong one and ruin my Mould etc, what is the polypropylene sheet for ( or is that the corrugated sign board ?) so again Thanks for all the help, Regards DM Hi Matt, another observation ??? looking at your Video Making the Bonnet Mould for the 27th time I suddenly realised you did not Vacuum Bag it and especially on the first layer over the Gel Coat which is the most important coat to make sure there was no air bubbles or voids under the gel, as I could understand no reason to VB any further layers, as the Mould is the most important piece to get spot on as hopefully you will be using for lots and lots of Mouldings ?? Regards DM Which kind of chopped strand matting do you have? Typically there is emulsion bound and powder bound. Epoxy lacks the solvents required to break down the emulsion binder, so we recommend the use of powder bound CSM as any resin will break the binder much easier. You will NOT need MEKP for our EL160 and EG160 as both are epoxy based and have their own specialist hardeners that need to be used. The polypropylene sheet is for use as a baseboard and to create flanges. Fluted signboard can be used to do the same thing albeit the surface finish is slightly ribbed compared to the perfectly smooth finish of pure polypropylene sheet.. Generally speaking, vacuum bagging is not needed for mould making. Wet lay mould making like suggested for your project is done without any vacuum bagging. As long as you pay careful attention to applying the gelcoat properly and the first layer of putty and glass, then you should not have any voids to worry about. You may be thinking of tooling pre-pregs, where depending on the system used and mould size, thickness etc, vacuum debulking may be necessary. Hi Warren, I do not know what type of CFM I have it is what I used for Fiberglassing ?? so how can I tell, it does not say on the label. I am just amazed that you do not recommend Vbing your Mould, as with my Airbox and the intricate Flange there is no way I could lay up and be sure I got all the air out and the Paste and Glass forced right into the very tight corners, as the last thing I want to be doing is trying to repair the Flange in my mould once released, a major nightmare, Regards DM
|