+x Dinoman - 7/15/2018 6:18:33 PM+x Steve Broad - 7/15/2018 6:07:05 PM+x Dinoman - 7/13/2018 8:41:57 PM+x Steve Broad - 7/13/2018 5:52:40 PM+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DMYes, it's my intake tube to the turbo. There is now a flange on the rectangle end to connect to the next section and a flange to bolt to the turbo.Hi Steve, Thanks, so was the rectangle end of your Mould blanked off for Vacuum bagging and then when released from mould you cut out the rectangle end, is that correct, again Thanks for your help, Regards DMNo, both ends were open and the bag was pushed in both ends and met in the middle.I Steve, I still cannot see how you can push one end of a bag in one end of your mould and the other end of your bag in the other end of your mold and have them meet in the middle, as far I can see when you Vacuumed your bag it would just colapse on it self so no pressure on the Molding ???Regards DM
+x Steve Broad - 7/15/2018 6:07:05 PM+x Dinoman - 7/13/2018 8:41:57 PM+x Steve Broad - 7/13/2018 5:52:40 PM+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DMYes, it's my intake tube to the turbo. There is now a flange on the rectangle end to connect to the next section and a flange to bolt to the turbo.Hi Steve, Thanks, so was the rectangle end of your Mould blanked off for Vacuum bagging and then when released from mould you cut out the rectangle end, is that correct, again Thanks for your help, Regards DMNo, both ends were open and the bag was pushed in both ends and met in the middle.
+x Dinoman - 7/13/2018 8:41:57 PM+x Steve Broad - 7/13/2018 5:52:40 PM+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DMYes, it's my intake tube to the turbo. There is now a flange on the rectangle end to connect to the next section and a flange to bolt to the turbo.Hi Steve, Thanks, so was the rectangle end of your Mould blanked off for Vacuum bagging and then when released from mould you cut out the rectangle end, is that correct, again Thanks for your help, Regards DM
+x Steve Broad - 7/13/2018 5:52:40 PM+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DMYes, it's my intake tube to the turbo. There is now a flange on the rectangle end to connect to the next section and a flange to bolt to the turbo.
+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DM
+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.
+x Steve Broad - 7/15/2018 8:55:37 PM+x Dinoman - 7/15/2018 6:18:33 PM+x Steve Broad - 7/15/2018 6:07:05 PM+x Dinoman - 7/13/2018 8:41:57 PM+x Steve Broad - 7/13/2018 5:52:40 PM+x Dinoman - 7/13/2018 3:20:07 PM+x Steve Broad - 7/13/2018 11:44:38 AMA bit like this.Hi Steve Thanks, I can see your mould has an opening on top, but is the other end also open like mine?? Regards DMYes, it's my intake tube to the turbo. There is now a flange on the rectangle end to connect to the next section and a flange to bolt to the turbo.Hi Steve, Thanks, so was the rectangle end of your Mould blanked off for Vacuum bagging and then when released from mould you cut out the rectangle end, is that correct, again Thanks for your help, Regards DMNo, both ends were open and the bag was pushed in both ends and met in the middle.I Steve, I still cannot see how you can push one end of a bag in one end of your mould and the other end of your bag in the other end of your mold and have them meet in the middle, as far I can see when you Vacuumed your bag it would just colapse on it self so no pressure on the Molding ???Regards DMYeah, I thought that at first, but it actually works :-) You suck the air out of the volume between the bag and the mould, regardless of what side the bag is. The air between the bag sections pushed into the openings is inside the bag so it is sucked out. Trust me, it works :-)