How do I Vaccum Bag this Air Box ??


Author
Message
Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Hi I have been looking at this Air Box and trying to figure out how I can Vaccum Bag ??? to me looks impossible, so any help appreciated, Regards DM
Attachments
458 Air Box.jpg (1.2K views, 1.00 MB)
Reply
Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Matt (Staff) - 7/20/2018 7:32:53 AM
Hi Dinoman,

To make sure everything all stays positive I think it's clear you've got a procedure in your mind that you want to follow and that's totally fine. In composites, I think we've all learned that there's usually several ways to achieve just about any task and each of us can only say what works for us.

From an Easy Composites perspective we tend to take things a little further and experiment with lots of different techniques so that we can provide added value to our customers (i.e. saving them from false starts) because we're less constrained in terms of resources, materials and expertise. We did do quite a bit of research (I'm talking hundreds of test panels) of vacuum bagging moulds for high temperature use and it didn't provide the benefits we were looking for (vacuum bagging doesn't eliminate the potential for air pockets between gel and reinforcement). Resin infusion - on the other hand - is a different story and resin infusing a mould does make a lot of sense and works well, however it's often impractical to do because you really need to be working on a solid pattern (either a splash part or tooling board) rather than an original with temporary barriers, etc.

I hope you the input from ourselves and other members useful, I'll be be interested to hear how you get on and of course be ready to learn something from your results.

All the best, Matt

Hi Matt, as you can see I am coming round to your way and everyone else's after Hanaldo pointed out the flaws in my thinking, so again Thanks for all your patience and a great Forum, Regards DM

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
                                 Trapped moulds, been there and got the relevant T-Shirt :-)
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
                                             Hi Steve, how can I tell if my fibreglass woven matt that has chemical binders ??, Regards DM
Dinoman - 8 Years Ago
     A bit like this.
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
                                                 Hi Thank, can you also tell me where I can download the data Sheets from as I tried the search box but it came back with nothing, Regards DM
Dinoman - 7 Years Ago
                                                     If you are talking about EC's component prepregs, click on the datasheet button on the details page.
Steve Broad - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
                 Hey eddie! Any updates on airbox?
Furkan Yahsi - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago