Hi I have been looking at this Air Box and trying to figure out how I can Vaccum Bag ??? to me looks impossible, so any help appreciated, Regards DM
Attachments
458 Air Box.jpg (1.2K views, 1.00 MB)
Replies
Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Hanaldo - 1/18/2019 5:25:05 PM
Yeh these sorts of epoxies are 100% solids - there are no solvents in them, and you cant add solvents to them. Only way to lower the viscosity is with heat.

Hi All again, Thanks for the advice, I will let you know how it turns out whether it is good or bad news, Regards DM

Eddie Walsh
E
Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)Supreme Being (542 reputation)
Group: Forum Members
Posts: 52, Visits: 294
Eddie Walsh - 1/18/2019 10:37:18 PM
Hanaldo - 1/18/2019 5:25:05 PM
Yeh these sorts of epoxies are 100% solids - there are no solvents in them, and you cant add solvents to them. Only way to lower the viscosity is with heat.

Hi All again, Thanks for the advice, I will let you know how it turns out whether it is good or bad news, Regards DM

Hi All, I have just spent most of the day trying to roll out the first layers of Mat on my mould ???, what it seemed like is the Epoxy Resin wasn't dissolving the Powder Binder in the Mat so I was just chasing large air pockets under my mat ?? eventually got it so it does not look too bad but definitely not perfect, I never had anything like this with Polyester, I suppose I was lucky temp was still low or it would have cured before I got it to a resonable state, again any help or advice appreciated, Regards DM

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
                                 Trapped moulds, been there and got the relevant T-Shirt :-)
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
                                             Hi Steve, how can I tell if my fibreglass woven matt that has chemical binders ??, Regards DM
Dinoman - 8 Years Ago
     A bit like this.
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
Warren (Staff) - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Steve Broad - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 8 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
                                                 Hi Thank, can you also tell me where I can download the data Sheets from as I tried the search box but it came back with nothing, Regards DM
Dinoman - 7 Years Ago
                                                     If you are talking about EC's component prepregs, click on the datasheet button on the details page.
Steve Broad - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
Dinoman - 8 Years Ago
Matt (Staff) - 8 Years Ago
Dinoman - 8 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Dinoman - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
                 Hey eddie! Any updates on airbox?
Furkan Yahsi - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
Dinoman - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
Matt (Staff) - 7 Years Ago
Dinoman - 7 Years Ago
oekmont - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search