That should be just a problem of using the wrong words/combination. There are eBay sellers for almost every weave you can think of. And for shure such common types.
Roving weaves are heavy cloth with whole rovings as threats. they are great to get a lot of reinforcement onto your laminate quickly, but they are not good as first layer, as they leave a texture through the tooling coat, because of their rough surface.
|