Group: Forum Members
Posts: 550,
Visits: 27K
|
How i do it: 166g Glass filament fabric for the first layer And then alternating between 600g roving fabric and 600g biaxial until the desired thickness is achieved.
If you first use putty all like mat suggests, the first lighter cloth should not be necessary. But a medium weight like 280 should be ideal to minimise print through. Everything with "Roving" in it's description should usually be to rough in it's texture. Except rovings itself... Everything with "mat" usually hints that there is some csm content, as far as i know. I advice a standard medium weight glass filament fabric. between 200 and 300g.
|