Hi, can anyone give advice on what is causing these air like bubbles are? any info would help. Thanks 

Reply
easby
easby
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 6, Visits: 44
Warren (Staff) - 12/5/2017 3:05:24 PM
It's hard to see in that photo.  Have you got any thing close up?



Not sure if this is any better??
They look like air bubbles but do not go with heat
Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
easby - 8 Years Ago
Warren (Staff) - 8 Years Ago
easby - 8 Years Ago
Warren (Staff) - 8 Years Ago
easby - 8 Years Ago
Warren (Staff) - 8 Years Ago
easby - 8 Years Ago
Interloper393 - 8 Years Ago
Warren (Staff) - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search