By easby - 12/5/2017 1:12:30 PM
Hi, can anyone give advice on what is causing these air like bubbles are? any info would help. Thanks
|
By Warren (Staff) - 12/7/2017 9:05:10 AM
If it is definitely pin holes then as described above, you can literally fill them before lacquering. Brushing into the pinholes is the way. You need the pinholes to fill up with lacquer before you move on.
|
|