Davidpetty1988
Davidpetty1988
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 89
Hi I'm doing resin infusion and I'm very happy with the glossy finish apart from some tiny gaps around the fibres on the surface finish.any ideas where I might be going wrong?
I hope its a clear enough picture thanks in advance
Dave
Tags
finish
Gaps
resin infusion
Reply
Like
9
Reply
Davidpetty1988
Davidpetty1988
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 89
So clamp the vac side first then leave the resin side pumping for another 20-30 secs then clamp the resin side off is this what you mean I read something like this in another post didn't no weather it was applicable to my problem.It quite confusing in the ec guide it tells you to do it another conflicting info.
Its a pretty glossy finish to be dry isn't it?
Edited
10 Years Ago by
Davidpetty1988
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Trouble with perfect finish
Davidpetty1988
-
10 Years Ago
hi, looks dry try leaving the resin side clamp off for longer.
VVS
-
10 Years Ago
So clamp the vac side first then leave the resin side pumping for another 20-30 secs then clamp the...
Davidpetty1988
-
10 Years Ago
It's dry. You have either clamped the resin too early, or you have allowed too much resin to be...
Hanaldo
-
10 Years Ago
Thanks very much guys will do that on my next peice . Dammit I love this forum site all you guys are...
Davidpetty1988
-
10 Years Ago
As previously said clamp the resin output line first and allow the vacuum in the bag to suck in some...
davro
-
10 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search