Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Resin Infusion
Trouble with perfect finish
http://www.talkcomposites.com/Topic20591.aspx
By Davidpetty1988
-
2/23/2016 12:53:20 PM
Hi I'm doing resin infusion and I'm very happy with the glossy finish apart from some tiny gaps around the fibres on the surface finish.any ideas where I might be going wrong?
I hope its a clear enough picture thanks in advance
Dave
By davro
-
2/24/2016 1:12:28 AM
As previously said clamp the resin output line first and allow the vacuum in the bag to suck in some resin before clamping the resin input line this should give you a nice resin rich part, without the pin holes
The clamping time can vary depending on the area of the sheet your pulling.