prsw
prsw
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 112,
Visits: 1K
Hi all
I plan to start with infusion now and one part I want to do has a mold
that I did some years ago when I only did wet layup, it has almost no flanges.
So I have to use an envelope bag, but is that possible with infusion?
Or will the resin go around the whole mold?
http://motoform.blogspot.se
Reply
Like
2
Replies
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
_GABBER
_GABBER
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 41,
Visits: 646
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then
this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
other side
final piece
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Thanks Gabber for the info!
looks great
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
1
prsw
prsw
posted 12 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 112,
Visits: 1K
_GABBER (18/01/2013)
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then
this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
Thanks again,
Can the feed spiral can be placed in the middle of the tool and stil spread the resin
as long as there is a dist-mesh with vacuum on either side?
So the resin does not flow, or very little beyond/outside the dist-mesh?
Do you get any resin on the back of the mold?
http://motoform.blogspot.se
Edited
12 Years Ago by
prsw
Reply
Like
1
_GABBER
_GABBER
posted 12 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 41,
Visits: 646
prsw (19/01/2013)
_GABBER (18/01/2013)
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then
this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
Thanks again,
Can the feed spiral can be placed in the middle of the tool and stil spread the resin
as long as there is a dist-mesh with vacuum on either side?
So the resin does not flow, or very little beyond/outside the dist-mesh?
Do you get any resin on the back of the mold?
I place the spiral in the midlle of the tool, and I infuse like the picture.
Resin flow a little outside the mesh, for my esperience about 3/4 cm, so I cut mesh smaller than the fiber.
I never had problems infusing like this.
On the back of the mold there is a little resin, but if you places well the bag, it's acceptable.
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Infusion on old mold without flanges
prsw
-
12 Years Ago
sounds quit difficult to do infusion without flanges... normaly you use your flanges for resin inlet...
matthieutje65
-
12 Years Ago
well, it has flanges but they are 15mm wide and have a very uneven surface, so it is not possible...
prsw
-
12 Years Ago
Envelope bag and you can infuse no problem.
Shaneer22
-
12 Years Ago
and how do you place your vacuum spiral tube and put the resin inlet?
matthieutje65
-
12 Years Ago
[quote][b]matthieutje65 (17/01/2013)[/b][hr]and how do you place your vacuum spiral tube and put the...
_GABBER
-
12 Years Ago
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral...
matthieutje65
-
12 Years Ago
[quote][b]matthieutje65 (18/01/2013)[/b][hr]Gabber, do you have smoe pictures of the set-up before...
_GABBER
-
12 Years Ago
Thanks Gabber for the info! looks great
matthieutje65
-
12 Years Ago
[quote][b]_GABBER (18/01/2013)[/b][hr][quote][b]matthieutje65 (18/01/2013)[/b][hr]Gabber, do you...
prsw
-
12 Years Ago
[quote][b]prsw (19/01/2013)[/b][hr][quote][b]_GABBER (18/01/2013)[/b][hr][quote][b]matthieutje65...
_GABBER
-
12 Years Ago
[quote][b]Shaneer22 (16/01/2013)[/b][hr]Envelope bag and you can infuse no problem.[/quote] Thank...
prsw
-
12 Years Ago
Thats interesting to know, I have a few molds without flnages that i thought we be no good for resin...
nutz
-
12 Years Ago
I just checked your site Petter, awesome work on the Cagiva Raptor. I used to race motorcycles too...
CompositeSeb
-
12 Years Ago
[quote][b]CompositeSeb (19/01/2013)[/b][hr]I just checked your site Petter, awesome work on the...
prsw
-
12 Years Ago
Subscribed to your RSS. Symmetry is such a pain when it comes to modeling. Very few tutorials or...
CompositeSeb
-
12 Years Ago
you can help the resin flow on the edges with a heat gun...or put before your mold in the oven, or...
_GABBER
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search