By prsw - 1/15/2013 8:32:17 PM				
            
                      
            Hi all
  I plan to start with infusion now and one part I want to do has a mold  that I did some years ago when I only did wet layup, it has almost no flanges. So I have to use an envelope bag, but is that possible with infusion? Or will the resin go around the whole mold?
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By _GABBER - 1/19/2013 2:39:50 PM				
            
                      
            you can help the resin flow on the edges with a heat gun...or put before your mold in the oven, or make a heated mold. I'm trying now a heated mold with RTMLight
           
		 | 			
		 
	
	
						
		 	
		
	 |