Hi all

I plan to start with infusion now and one part I want to do has a mold
that I did some years ago when I only did wet layup, it has almost no flanges.
So I have to use an envelope bag, but is that possible with infusion?
Or will the resin go around the whole mold?


http://motoform.blogspot.se

Replies
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
_GABBER (18/01/2013)
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then


this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
http://www.talkcomposites.com/Uploads/Images/eabde875-fe3b-415e-a5b2-3f7f.JPG


Thanks again,
Can the feed spiral can be placed in the middle of the tool and stil spread the resin
as long as there is a dist-mesh with vacuum on either side?

So the resin does not flow, or very little beyond/outside the dist-mesh?
Do you get any resin on the back of the mold?


http://motoform.blogspot.se

Edited 12 Years Ago by prsw
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
prsw (19/01/2013)
_GABBER (18/01/2013)
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then


this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
http://www.talkcomposites.com/Uploads/Images/eabde875-fe3b-415e-a5b2-3f7f.JPG


Thanks again,
Can the feed spiral can be placed in the middle of the tool and stil spread the resin
as long as there is a dist-mesh with vacuum on either side?

So the resin does not flow, or very little beyond/outside the dist-mesh?
Do you get any resin on the back of the mold?








I place the spiral in the midlle of the tool, and I infuse like the picture.
Resin flow a little outside the mesh, for my esperience about 3/4 cm, so I cut mesh smaller than the fiber.
I never had problems infusing like this.
On the back of the mold there is a little resin, but if you places well the bag, it's acceptable.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 12 Years Ago
matthieutje65 - 12 Years Ago
prsw - 12 Years Ago
Shaneer22 - 12 Years Ago
matthieutje65 - 12 Years Ago
_GABBER - 12 Years Ago
matthieutje65 - 12 Years Ago
_GABBER - 12 Years Ago
                             Thanks Gabber for the info! looks great
matthieutje65 - 12 Years Ago
prsw - 12 Years Ago
                                 [quote][b]prsw (19/01/2013)[/b][hr][quote][b]_GABBER (18/01/2013)[/b][hr][quote][b]matthieutje65...
_GABBER - 12 Years Ago
prsw - 12 Years Ago
nutz - 12 Years Ago
CompositeSeb - 12 Years Ago
prsw - 12 Years Ago
CompositeSeb - 12 Years Ago
_GABBER - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search