Hi all

I plan to start with infusion now and one part I want to do has a mold
that I did some years ago when I only did wet layup, it has almost no flanges.
So I have to use an envelope bag, but is that possible with infusion?
Or will the resin go around the whole mold?


http://motoform.blogspot.se

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
sounds quit difficult to do infusion without flanges...
normaly you use your flanges for resin inlet and or vacuumport.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
well, it has flanges but they are 15mm wide and have a very uneven surface,
so it is not possible to seal a bag with gumtape, but it might do the other jobs.


http://motoform.blogspot.se

Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Envelope bag and you can infuse no problem. 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
and how do you place your vacuum spiral tube and put the resin inlet?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Shaneer22 (16/01/2013)
Envelope bag and you can infuse no problem. 


Thank you.


http://motoform.blogspot.se

_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
matthieutje65 (17/01/2013)
and how do you place your vacuum spiral tube and put the resin inlet?




you place vacuum spiral tube into the bag all around the mold, no problem if it isn't fixed with the mold. I did many times like this 
nutz
nutz
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 58
Thats interesting to know, I have a few molds without flnages that i thought we be no good for resin infusion. Wont have to chuck em away and start again now
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
matthieutje65 (18/01/2013)
Gabber, do you have smoe pictures of the set-up before infusion? quit curious about how the spiral is layed around then


this is a carbon fibre mold made with resin infusion. If you look around you see the vacuum spiral
http://www.talkcomposites.com/Uploads/Images/eabde875-fe3b-415e-a5b2-3f7f.JPG


http://www.talkcomposites.com/Uploads/Images/38928a9f-e2e5-428c-9782-74fb.JPG


other side
http://www.talkcomposites.com/Uploads/Images/e088d726-2014-41a8-ab27-8a10.JPG




final piece 
http://www.talkcomposites.com/Uploads/Images/1e7f3ad9-c11e-4050-9739-8656.JPG