Phat13
Phat13
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 138
Hi guys, I'm about to try my first infusion ,
It's a small cafe racer seat with a lot of shape
Can I cut the peel ply to lay it neater or is it ok to have big folds in it
Thanx in advance
Wayne :0)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Peel ply question
Phat13
-
12 Years Ago
Both are fine, it's porous so makes no real difference. The only issue with cuts is sometimes it can...
ajb100
-
12 Years Ago
Thank you buddy, That's cool then as I recon it will make it easier for me. Cheers Wayne :0)
Phat13
-
12 Years Ago
I had an issue once there I tried laying it with folds in it, and I didn't realise it actually...
Hanaldo
-
12 Years Ago
Yes I have now made a pattern so I can cut the infusion mesh an peel ply, I'm finding it very...
Phat13
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search