Phat13
Phat13
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 11,
Visits: 138
Yes I have now made a pattern so I can cut the infusion mesh an peel ply, I'm finding it very hard,it's almost likea bowl I'm having to lay all the bits in ,ha ha not easy as I discover !
Reply
Like
3
Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I had an issue once there I tried laying it with folds in it, and I didn't realise it actually pinched a small amount of carbon fibre in one of the folds. Of course when that infused and cured, it mechanically locked the peel ply in place so I ended up with this shred of peel ply permanently stuck in the part. Ended up binning it.
These days I always cut the peel ply so that it lays flat on the surface. I put perforated release film over the top so that I can remove it all easier come demould.
Reply
Like
2
Phat13
Phat13
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 11,
Visits: 138
Thank you buddy,
That's cool then as I recon it will make it easier for me.
Cheers
Wayne :0)
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Both are fine, it's porous so makes no real difference. The only issue with cuts is sometimes it can tear along the cut and be a pain to removed
Reply
Like
3
Phat13
Phat13
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 138
Hi guys, I'm about to try my first infusion ,
It's a small cafe racer seat with a lot of shape
Can I cut the peel ply to lay it neater or is it ok to have big folds in it
Thanx in advance
Wayne :0)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search