Hi guys, I'm about to try my first infusion ,
It's a small cafe racer seat with a lot of shape
Can I cut the peel ply to lay it neater or is it ok to have big folds in it
Thanx in advance
Wayne :0)
By Phat13
-
3/24/2014 7:15:07 PM
Yes I have now made a pattern so I can cut the infusion mesh an peel ply, I'm finding it very hard,it's almost likea bowl I'm having to lay all the bits in ,ha ha not easy as I discover !