Hi guys, I'm about to try my first infusion ,
It's a small cafe racer seat with a lot of shape

Can I cut the peel ply to lay it neater or is it ok to have big folds in it

Thanx in advance 

Wayne :0)
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Both are fine, it's porous so makes no real difference. The only issue with cuts is sometimes it can tear along the cut and be a pain to removed
Phat13
Phat13
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 11, Visits: 138
Thank you buddy,
That's cool then as I recon it will make it easier for me. 

Cheers
Wayne :0)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I had an issue once there I tried laying it with folds in it, and I didn't realise it actually pinched a small amount of carbon fibre in one of the folds. Of course when that infused and cured, it mechanically locked the peel ply in place so I ended up with this shred of peel ply permanently stuck in the part. Ended up binning it. 

These days I always cut the peel ply so that it lays flat on the surface. I put perforated release film over the top so that I can remove it all easier come demould. 
Phat13
Phat13
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 11, Visits: 138
Yes I have now made a pattern so I can cut the infusion mesh an peel ply, I'm finding it very hard,it's almost likea bowl I'm having to lay all the bits in ,ha ha not easy as I discover !