Hi,




I need to do a CF roof to a Civic, but I do not know how many layers have to be applied.

In the car, it will be mounted a rollbar, so I think that the roof does not need to be very strong.




Pedro
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Is it for completion or road use?
pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
It´s for competition.