Hi,




I need to do a CF roof to a Civic, but I do not know how many layers have to be applied.

In the car, it will be mounted a rollbar, so I think that the roof does not need to be very strong.




Pedro
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I've just done a roof.  Mine is 2x200g/3mm PVC foam core/2x200g.  Its not absolutely rigid but its still pretty dam close.  I'd expect that something bonded around its entire perimiter would be fine in this layup.