By pedcrist - 11/16/2013 11:14:53 PM
Hi,
I need to do a CF roof to a Civic, but I do not know how many layers have to be applied.
In the car, it will be mounted a rollbar, so I think that the roof does not need to be very strong.
Pedro
|
By FLD - 11/19/2013 3:42:48 PM
Ah yes, thats a fair point raised there! I had to slot the foam for the areas where the curvature was greater. 3D core or soric would be easier for that.
|
|