Hi,




I need to do a CF roof to a Civic, but I do not know how many layers have to be applied.

In the car, it will be mounted a rollbar, so I think that the roof does not need to be very strong.




Pedro
Reply
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
FLD (19/11/2013)
Thats interesting as I favour foam over soric.  I guess personal preference plays its part.  3D core is also pretty good. 
Hi
I don't claim that pvc is worse but  I prefer soric because it is like fabric and pvc foam is... foam, and on flat, not demanding surface like dashboard switch pannel foam is better, but  I wouldn't use foam while doing hood or roof. But this is only my opinion BigGrin

~~~Everytime I hear sound of demoulding part I have eargasm~~~
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search