I am new here and have had a quick look through the forums and on the easy composites website/videos and I have yet to see any real advanced techniques shown (please correct me if I'm wrong and there is in fact advanced tutorials somewhere that state the techniques that I am referring to).

I have personally had over 10 years experience working with all aspects of advanced composites and the family run company that I own has been in the business for over 30 years. We have worked mostly in marine but have covered all aspects along the way from F1 through to aerospace.

I thought that I would list just a few things here and people can maybe carry this on and extend any knowledge/tips they may have learnt along the way.

To start with, no matter what composite project you are working on, it is all in the preparation, it is the most important thing. I.e, cutting materials correctly and all consumables ready to go before you even think about getting started. Working cleanly is also very important and something you learn working professionally within the industry. I will post some of my top tips of preparation and working cleanly later on this thread.

For now a couple of advanced pre-preg tips:

Spike rollers - I have not seen these listed anywhere on this forum or the main site, if you do not know what I refer to, it is basically a roller with spikes sticking out. It is important to spike roller each layer of pre-preg that you put down in the stack as this creates small holes within the otherwise solid resin structure for any air pockets to escape during debulking.

Debulking - As a general rule of thumb you should always debunk every 2 layers, along with the spike roller this gets rid of air pockets trapped in the stack and helps 'set' the pre-preg in place as you go.

Breather tows - A breather toe is simple a short tow of fibreglass placed around the edge of the laminate (in the area to be trimmed), you should place one tow roughly every 250-500mm for large panels/mouldings and smaller distances apply for smaller jobs. This is more important with infusion and Sprint system pre-pregs as it enables the air to escape more easily between layers but also applies to pre-preg as well if you want to do a professional job.

Pre-preg curing - I have had a quick look through the easy composites pre-preg offering and was surprised to find fairly basic information regarding the resin systems used and the cure process. Not anywhere mentioned is the recommended ramp rate for cure which is extremely important. As a general rule of thumb anywhere from 0.3C to 2C per minute is acceptable but this really depends on the application and should be specified by the manufacturer. Ramp rates allow the resin to flow correctly eliminating pin holes and voids and it allows the cured resins tg1 to stay ahead of the 'cure'.

Dwell times - A dwell is a temperature hold for a set period of time in order for the stack and mould to catch up with the rest of the cure, this all depends on the oven and should be analysed using oven test before curing any pre-preg. Once you have learnt your oven you can apply this to all future cures and can set an appropriate dwell time.

That concludes just a few things that I have noticed were never mentioned thus far. I am working on a very detailed pre-preg guide which will include many tips and goes into extreme detail in order to achieve results seen in the most advanced racing yachts/f1/aerospace applications. Please let me know if you are interested in this.

Please feel free to add any other advanced suggestions on working with pre-pregs and I will post more up when I have time.

Thanks and I hope this helps anyone interested.
Replies
mawgan
mawgan
Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)
Group: Forum Members
Posts: 12, Visits: 32
Hi Fred,

Thanks for your question. I will take a photo of the spike rollers that we use and put it up this week, I'm not sure exactly where you can buy them from as we order through a company called Monks & Crane who supply all of our workshop consumables (like rollers and handles etc) but there must be an online retailer that will sell them.

I have also attached some photos of some Carbon fibre skateboards that I have produced, they utilise a vertically laminated bamboo core with Carbon fibre/glass fibre composite and we mill them on our CNC machine. The boards in the photos are produced using wet layup, I have also made them with pre-preg, etc.

Thanks.

Mawgan.
Attachments
speedboard 38_2.jpg (676 views, 282.00 KB)
pintail 40.jpg (616 views, 275.00 KB)
speedboard 38.jpg (685 views, 278.00 KB)
speedboard 38.jpg (615 views, 278.00 KB)
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
mawgan (01/09/2013)
Hi Fred,

Thanks for your question. I will take a photo of the spike rollers that we use and put it up this week, I'm not sure exactly where you can buy them from as we order through a company called Monks & Crane who supply all of our workshop consumables (like rollers and handles etc) but there must be an online retailer that will sell them.

I have also attached some photos of some Carbon fibre skateboards that I have produced, they utilise a vertically laminated bamboo core with Carbon fibre/glass fibre composite and we mill them on our CNC machine. The boards in the photos are produced using wet layup, I have also made them with pre-preg, etc.

Thanks.

Mawgan.


Your boards like very nice.
Fred

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mawgan - 13 Years Ago
wozza - 13 Years Ago
mawgan - 13 Years Ago
wozza - 13 Years Ago
mawgan - 13 Years Ago
compositepro - 13 Years Ago
andygtt - 13 Years Ago
Shaneer22 - 13 Years Ago
Warren (Staff) - 13 Years Ago
morepower - 13 Years Ago
carboncactus - 13 Years Ago
morepower - 13 Years Ago
wozza - 13 Years Ago
compositepro - 13 Years Ago
Warren (Staff) - 13 Years Ago
morepower - 13 Years Ago
                 [quote][b]morepower (22/08/2013)[/b][hr]...
carboncactus - 13 Years Ago
morepower - 13 Years Ago
andygtt - 13 Years Ago
morepower - 13 Years Ago
wozza - 13 Years Ago
morepower - 13 Years Ago
TomDesign - 13 Years Ago
morepower - 13 Years Ago
TomDesign - 13 Years Ago
morepower - 13 Years Ago
morepower - 13 Years Ago
TomDesign - 13 Years Ago
fgayford - 13 Years Ago
mawgan - 13 Years Ago
fgayford - 13 Years Ago
Airship-Jim - 13 Years Ago
Airship-Jim - 13 Years Ago
morepower - 13 Years Ago
TomDesign - 13 Years Ago
morepower - 13 Years Ago
mawgan - 12 Years Ago
FLD - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search