Most CNC routers should be able to cut carbon sheet in 1mm dead easily. PCB cutters work very well for this purpose and are cheap and easily sourced and replaced when they get blunt.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Rogier Claes
Rogier Claes
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 3, Visits: 39
I've been looking around for a CNC cutter/laser to cut out certain standard shapes. We mainly use xpreg XC 110 and XC 130 (unidirectional). I came across the CNC-step machines. On their site it says they can cut prepreg with an oscillating knive, but in reality it turns out there are some issues. Does anyone know of a system or manufacturer that allows CNC cutting of prepreg materials?

Rogier
Edited 6 Years Ago by Rogier Claes
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search