By Rogier Claes - 8/26/2019 11:14:42 AM
I've been looking around for a CNC cutter/laser to cut out certain standard shapes. We mainly use xpreg XC 110 and XC 130 (unidirectional). I came across the CNC-step machines. On their site it says they can cut prepreg with an oscillating knive, but in reality it turns out there are some issues. Does anyone know of a system or manufacturer that allows CNC cutting of prepreg materials?
Rogier
|
By Kairu - 5/14/2020 2:05:04 AM
My work uses ultrasonic blades to cut prepreg even then after a while they need to changed or cleaned from the resin
|
|