depends on surface finish and how much resin you want to soak up, as it sounds like a large flat sheet of material it should be a simple enough infusion however it is a thick laminate so you will need to ensure that your chosen resin system will infuse the whole stack. What infusion consumables do you have? Infusion mesh / MTI hose?
|