+x scottracing - 3/5/2019 6:37:54 PMwhy have you got peel ply on both sides?
+x scottracing - 3/5/2019 7:52:46 PMdepends on surface finish and how much resin you want to soak up, as it sounds like a large flat sheet of material it should be a simple enough infusion however it is a thick laminate so you will need to ensure that your chosen resin system will infuse the whole stack.What infusion consumables do you have? Infusion mesh / MTI hose?