Project Showroom


Author
Message
DerekKarbonWorx
DerekKarbonWorx
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 13
Deyan Georgiev
Deyan Georgiev
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 2, Visits: 65
Hi everyone Smile

 this is some of the projects i've done:

1 air duct/vent? there was some pin holes and gaps on the front edges but as first time (total beginer) doing something like that i was happy Smile

and second reply for the other pictures BigGrin! ran out of space !
Attachments
5.JPG (881 views, 188.00 KB)
7.JPG (852 views, 1.00 MB)
8.JPG (703 views, 1.00 MB)
12.JPG (781 views, 175.00 KB)
14.JPG (805 views, 151.00 KB)
17.JPG (780 views, 208.00 KB)
18.JPG (815 views, 192.00 KB)
19.JPG (789 views, 136.00 KB)
21.JPG (797 views, 290.00 KB)
20.JPG (784 views, 234.00 KB)
28.JPG (752 views, 309.00 KB)
30.JPG (792 views, 259.00 KB)
33.JPG (831 views, 286.00 KB)
Brucecreations
Brucecreations
Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)Supreme Being (476 reputation)
Group: Forum Members
Posts: 25, Visits: 371
My last project about carbon fiber in the fashion field

For more in this forum  Carbon fiber and fashion


https://i37.servimg.com/u/f37/13/17/52/45/brascc10.jpg

https://i37.servimg.com/u/f37/13/17/52/45/esposi10.jpg

https://i37.servimg.com/u/f37/13/17/52/45/valigi14.jpg





My You Tube Channel
Edited 10 Years Ago by Brucecreations
scottracing
scottracing
Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
I dont usually post up my work as its usually customer projects that are secret and not that interesting to look at but this is.
Anew didabled sitski that we designed and built in under 3 months. Was good to get back on the tools and laminate the structural parts and bodywork.
Attachments
IMG-20170320-WA0000.jpg (864 views, 184.00 KB)
Lewismotorsport
Lewismotorsport
Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)
Group: Forum Members
Posts: 4, Visits: 32
hi bruce, what are you using as a mould to get that near full circle? i would have use for a similar looking part that is much longer and would wrap aroud a roll cage, also how did you manage to get the honeycomb to come out so well through the carbon?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
For a few years now Easy Composites have been working with the Antakari Solar Team in Chile, supplying all the composite materials for their Intikallpa solar car. They compete in the World Solar Challenge. A few weeks back our good friend at the team, Daniel Garrido, sent through some photos of the car when it arrived safely at Hidden Valley Motor Sport in Darwin, Australia. Daniel and the team make extensive use of carbon fibre composites in the body construction, primary using epoxy resin infusion and of course all composite materials supplied by us Smile
You can see the spread-tow carbon fibre used on the sandwich panel internal bulkheads in this photo:

The main body of the car is all done in carbon fibre composites too. You might just make out the Easy Composites logo on the side of the car. Thanks guys Smile

We wish the whole of the Antakari team the best of luck with the car. If you'd like to find out more about the car, the team or the series, you'll find them at:

Antakari Solar Team (Facebook): @proyectointikallpa
AntakariST (Twitter): @AntakariST
Intikallpa_chile (Instagram)
www.Intikallpachile.cl (web page)


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 9 Years Ago by Matt (Staff)
Jossure
J
Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)Supreme Being (101 reputation)
Group: Forum Members
Posts: 6, Visits: 17
I just started designing on computer about 3 weeks ago and I would like to hear your opinions on this project that I am working on. My goal is to create a great design then go all in and make it from scratch. But so far this is all I have learned in 3 weeks. Please leave your comment. 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It depends how far you want to go on the design side.  You could design every panel and item or just use the shape to get a solid model to cut a foam buck from then do the rest separately.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Frank
Frank
Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)Supreme Being (384 reputation)
Group: Forum Members
Posts: 27, Visits: 123
First project, 4th demoulded part:


after demould


and with dekor
Regards
Frank

Edited 8 Years Ago by Frank
Ken Olson
Ken Olson
Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)Supreme Being (114 reputation)
Group: Forum Members
Posts: 8, Visits: 41
Here are a couple of my carbon fiber RC boats. All carbon fiber 54-55 inches long. 12 inch G.I. Joe driver. 
 