mannime
mannime
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 31
Hi guys,
I plan to do a resin infusion as follows: (top to bottom)
bagging film (from starter pack)
160g twill weave
390g twill weave
closed cell foam
390g twill weave
160g twill weave
flat acrylic mould (perspex)
As this is first time I'm going to do this I'm worried if the finished product will be shiny, smooth and glossy on both sides? Or I am missing something here?
Thank you
Reply
Like
3
Replies
mannime
mannime
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 31
Rob, could give me an explanation as to why infusion wouldn't work with closed cell foam ?
Reply
Like
2
r0bsk1
r0bsk1
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 38,
Visits: 307
The closed cell foam would act as a barrier to the resin and it will not penetrate the layers of carbon against the mold.
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I have to say, i've worked with closed cell foam and it worked for me...
There's a thing with the plexiglass, perspex, pmma,... :p that could cause a problem...
I've once did an infusion on a flat piece of plexiglass, Due to the resin getting hot when reacting it melted the plexiglass into the piece,
making it a difficult to remove even with the mouldrelease applied on it, had to remove it with a heatgun...
But just like robsk1 says just do some testsamples to see how it works for you, maybe I just had some good/bad luck with the closed cell foam and plexiglass.
good luck!
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
mannime
mannime
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 31
Hi Matthieu,
now I'm worried about my plexiglass surface. Any suggestions as to what else I could use? I need as flat surface as possible, to avoid any additional sanding and polishing on the part.
Thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Shiny on both sides
mannime
-
13 Years Ago
With a standard infusion process you'll need to use a flow media and peel ply to enable the removal...
r0bsk1
-
13 Years Ago
Rob, thanks for your reply. Well I cannot use another perspex on top, because the top surface will...
mannime
-
13 Years Ago
Yes, you'll get a shine off the bagging material but it'll be nothing like what you'd get from a...
r0bsk1
-
13 Years Ago
Rob, could give me an explanation as to why infusion wouldn't work with closed cell foam ?
mannime
-
13 Years Ago
The closed cell foam would act as a barrier to the resin and it will not penetrate the layers of...
r0bsk1
-
13 Years Ago
I have to say, i've worked with closed cell foam and it worked for me... There's a thing with the...
matthieutje65
-
13 Years Ago
Hi Matthieu, now I'm worried about my plexiglass surface. Any suggestions as to what else I could...
mannime
-
13 Years Ago
Glass sheet, needs to be a good quality toughened glass, and not laminated. Ideally automotive glass...
pk_090
-
13 Years Ago
Mirrors work out great too check this video I've made me making some testsamples....
matthieutje65
-
13 Years Ago
Hi Matthieu, thanks for sharing that video. I'm really interested in your test results. Do you...
mannime
-
13 Years Ago
Well I did this for personal use, to add to my "material library" I haven't tested them in a lab or...
matthieutje65
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search