By mannime - 7/3/2012 1:01:24 PM

Hi guys,

I plan to do a resin infusion as follows: (top to bottom)

bagging film (from starter pack)
160g twill weave
390g twill weave
closed cell foam
390g twill weave
160g twill weave
flat acrylic mould (perspex)

As this is first time I'm going to do this I'm worried if the finished product will be shiny, smooth and glossy on both sides? Or I am missing something here?

Thank you
By matthieutje65 - 7/6/2012 12:24:28 PM

Well I did this for personal use, to add to my "material library" I haven't tested them in a lab or something like that so I don't have numbers about their stiffness and strenght.
What I can say is that the PVC foam cored sample is quit strong in ratio to his weight.
A second remarkable thing was the carbonfiber sandwich with fiberglass. I've did Carbon-glas-Carbon-glas-Carbon resulting in a very stiff, but heavier part. 
samples with the carbon only start to get stiff after 5+ layers. When there are less layers its quit easy to bend.