I use the IN2 infusion resin, can I degass half a cup with the infusion catch pot? Or is the catchpot to small and it will be messy?
Reply
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
Well, it did get messy Smile But only because I opened the vent valve to fast... Its no problem to degass as long as you only degas 150g or less. If you try more than this the cup is to small, and there will get messy. 