Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Degassing with the catchpot?
Degassing with the catchpot?
Post Reply
Like
2
Degassing with the catchpot?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I use the IN2 infusion resin, can I degass half a cup with the infusion catch pot? Or is the catchpot to small and it will be messy?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Degassing with the catchpot?
67redrocket
-
10 Years Ago
will probably get messy, can expand up to 4 times in mass sometimes, depending on the temperature of...
matthieutje65
-
10 Years Ago
Never tried or thought about it but I cannot see why it wouldn't work. Can't see it being any...
davro
-
10 Years Ago
Well, it did get messy :) But only because I opened the vent valve to fast... Its no problem to...
67redrocket
-
10 Years Ago
Yeh be careful using the catch pot, I destroyed an expensive vacuum gauge attempting to degas 100ml...
Hanaldo
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search