By 67redrocket - 1/7/2016 6:47:51 AM
I use the IN2 infusion resin, can I degass half a cup with the infusion catch pot? Or is the catchpot to small and it will be messy?
|
By Hanaldo - 1/12/2016 12:10:15 PM
Yeh be careful using the catch pot, I destroyed an expensive vacuum gauge attempting to degas 100ml of resin in a 450ml cup
|
|