67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I use the IN2 infusion resin, can I degass half a cup with the infusion catch pot? Or is the catchpot to small and it will be messy?
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
will probably get messy, can expand up to 4 times in mass sometimes, depending on the temperature of the resin and how many air is trapped in it
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Never tried or thought about it but I cannot see why it wouldn't work.
Can't see it being any messier than using a full size degasser.
I only degas half cups at a time in my large degasser to ensure the cup never overflows and makes a mess in the bucket in the degasser, granted your going to be working in tight catch pot space, but all your doing is applying a vaccum to some resin.
Would be interesting experiment to try.
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
10 Years Ago by
davro
Reply
Like
3
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 486
Well, it did get messy
But only because I opened the vent valve to fast... Its no problem to degass as long as you only degas 150g or less. If you try more than this the cup is to small, and there will get messy.
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yeh be careful using the catch pot, I destroyed an expensive vacuum gauge attempting to degas 100ml of resin in a 450ml cup
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search