Group: Forum Members
Posts: 67,
Visits: 910
|
I mixed the resin with slow hardner, I didn't have any blow heaters on it was done in the house, the places where it had collapsed were at the barb on the pump, where it entered the catch pot and where I'd previously had it clamped for drop test
|