autoclave


Author
Message
Greg
Greg
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 7, Visits: 353
f1rob (16/05/2014)
As long as you have 1vac line going in and a gauge linked to the system that's all you need to start with it can be VERY basic and will work 99% as well as an all singing all dancing pc controlled clave

All depends what you want to do and how much you want to spend


I want 3 or  4 vac line, at this moment I have tri-angle pipe line at oven but IMO it was't good idea. I mean 3  gauges. 
http://www.talkcomposites.com/Uploads/Images/9f49dea9-594b-42fd-b054-bb86.jpg
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Not a bad effort from the second example lot of work gone into it wish I could read it

Hope the water coming out was after a successful pressure test and not during !

Nod sure I would go with the round heating elements that size vessel your heat distribution is going to be good even without a fan and there is an awful lot of fire risk with a 360 deg coverage of elements

lot better on the bottom with a cover
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
I have seen a homemade autoclave made from a propane bottle, about 1m long and 35cm diameter. Unfortunately the forum this was posted in doesn't exist anymore, I only have two pictures:






Another homebuilt autoclave:

http://www.stonebock.ch/Stonebock/Autoklav.html
http://www.stonebock.ch/Stonebock/Fotos_Autoklav.html
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
As long as you have 1vac line going in and a gauge linked to the system that's all you need to start with it can be VERY basic and will work 99% as well as an all singing all dancing pc controlled clave

All depends what you want to do and how much you want to spend
Greg
Greg
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 7, Visits: 353
Do you know where I can buy maniold system for autoclave?
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
As you dont want an opinion on buying or not buying. I will just say get one with an interlocking door not a bolt fixture one. The last thing you want is the bolts letting go and an exploding autoclave door...

You will need to make sure it has a good manifold system and controllers to allow for pressure increases as the temp rises.. basic ones do not do this with the controller and you may have to vent excess pressure manually.. 
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
ajb100 (08/03/2014)
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers


appreciate your input but i didnt ask for opinions on whether i should buy one or not Wink
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
i know theyre pretty damn pricy, just that when it comes to me and sourcing expensive equipment i usually end up finding the worst product ha
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search