Hi guys
does anyone know where to get smaller sized autoclaves, from say .5m3 to 1m3?
By Greg - 5/21/2014 1:16:36 PM

f1rob (16/05/2014)
As long as you have 1vac line going in and a gauge linked to the system that's all you need to start with it can be VERY basic and will work 99% as well as an all singing all dancing pc controlled clave

All depends what you want to do and how much you want to spend


I want 3 or  4 vac line, at this moment I have tri-angle pipe line at oven but IMO it was't good idea. I mean 3  gauges. 
http://www.talkcomposites.com/Uploads/Images/9f49dea9-594b-42fd-b054-bb86.jpg