Group: Forum Members
Posts: 237,
Visits: 4.8K
|
As long as you have 1vac line going in and a gauge linked to the system that's all you need to start with it can be VERY basic and will work 99% as well as an all singing all dancing pc controlled clave
All depends what you want to do and how much you want to spend
|