Hi guys
does anyone know where to get smaller sized autoclaves, from say .5m3 to 1m3?
Reply
Like
2
Reply
coleio
coleio
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 68,
Visits: 285
ajb100 (08/03/2014)
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers
appreciate your input but i didnt ask for opinions on whether i should buy one or not
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
autoclave
coleio
-
11 Years Ago
You can get medical autoclave but even they are a few grand
ajb100
-
11 Years Ago
i know theyre pretty damn pricy, just that when it comes to me and sourcing expensive equipment i...
coleio
-
11 Years Ago
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most...
ajb100
-
11 Years Ago
[quote][b]ajb100 (08/03/2014)[/b][hr]Unless you're making top end components, you don't need an...
coleio
-
11 Years Ago
As you dont want an opinion on buying or not buying. I will just say get one with an interlocking...
morepower
-
11 Years Ago
Do you know where I can buy maniold system for autoclave?
Greg
-
11 Years Ago
As long as you have 1vac line going in and a gauge linked to the system that's all you need to start...
f1rob
-
11 Years Ago
[quote][b]f1rob (16/05/2014)[/b][hr]As long as you have 1vac line going in and a gauge linked to the...
Greg
-
11 Years Ago
I have seen a homemade autoclave made from a propane bottle, about 1m long and 35cm diameter....
brainfart
-
11 Years Ago
Not a bad effort from the second example lot of work gone into it wish I could read it Hope the...
f1rob
-
11 Years Ago
http://www.microsofttranslator.com/bv.aspx?from=&to=en&a=http://www.stonebock.ch/Stonebock/Autoklav....
brainfart
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search