autoclave


Author
Message
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
Hi guys
does anyone know where to get smaller sized autoclaves, from say .5m3 to 1m3?
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
ajb100 (08/03/2014)
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers


appreciate your input but i didnt ask for opinions on whether i should buy one or not Wink