Very Very Nice. I particularly like those hinges, art and engineering beautifully combined.Smile

Warren

Carbon Copies Ltd
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
great job Joe!

You've made some great decisions and I must say I would have done it exactly as you did!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Got nothing interesting and shiny ATM, but recently started on making some carbon fibre wheels for an Eco racer. This is the first one nearly ready for testing to ensure its strong enough! The bodywork when I get to it will also be a combination of carbon fibre, jute and flax which I'm quite looking forward to.



wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Nice to see something different. Keep us updated on progress.Smile

Warren

Carbon Copies Ltd
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Little update. It passed the lateral load test with flying colours today, to the point I'm re evaluating the layup schedule for them as it now seems excessive.

The clamps are to simulate it being bonded together at the outer edge as I haven't done that yet. Each wheel with tyre weigh 19kg and there was minimal deflection. I expect it to get even stronger when it is fully bonded



wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Excellent. I misread the post at first, I thought you were saying the carbon wheel weighed in at 19kgSmile Thought that cant be right.

Warren

Carbon Copies Ltd
Edited 12 Years Ago by wozza
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Haha, not that much thankfully. I haven't actually weighed it yet, will wait again until it's bonded to get an accurate idea.
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Are you involved in the whole project or just the wheels? This is what I love about this business you never know whats coming through the door next. Keeps life interestingSmile

Warren

Carbon Copies Ltd
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Make the compomotives in carbon!! you know you want to! Wink

Would be interesting to experiment with a full sized wheel.  Only a few manufacturers make them and they are very tight lipped about the processes used to get it to work.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I'm involved with the whole project, including the chassis building and geometry design. I'm really looking forward to the body work though as part of the Eco theming we'll be using as much flax and jute as possible

It certainly does, when I started I was just doing little ducts and bits for cars, but I've since worked with a prosthetic part and tea trays, you never know what's coming.

The compos could definitely do with being carbon, they weigh a ton. The person who got me interested in composites and taught me the basics was a guy called Steve Thomas who worked for Dymag and did a lot with their motorbike wheels. I don't the the full process but he showed me the inflatable bladder he had for making the spoked section of the wheel.

We also have a Dymag rim which was part of a two piece wheel, the outer being carbon and the face being alloy