Couldn't make it down myself but waiting on the feedback and any photos and video (he was under strict instructions to GoPro the lot)
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Looking good. How did the testing go yesterday ?

Warren

Carbon Copies Ltd
ChrisR
ChrisR
Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)Supreme Being (4.7K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Finished this on Tuesday night, tested on the water on Wednesday and hopefully down the cable park on Sunday. (Not me riding though, it's one of the British Team riders)


As it's a proof of concept you'll have to excuse the wrinkles and the pin holes!



It's a mix of all carbon 300 Bi-ax, 375 2/2 Twill, 6mm M80 core, carbon stringers with a bit of 650 in places and 200gsm on the footpads with a peel ply finish to add traction
Tags
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
The regs for our car require a minimum 1.5 body thickness around the driver, so a layer of carbon either side the 600g flax will be used to to bulk out these areas
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Got pictures of any of that work Warren? Those fabrics have interested me for some around-the-house objects that I was thinking of making...
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Warren (Staff) (04/04/2014)
I do find the use of jute and flax a bit of a false economy especially if your part needs some stiffness to it.  Both are very weak fabrics compared to carbons, so any environmental credentials are wiped out because you need to use more layers and as a consequence, more harmful resins to wet out the laminate.


Have to agree on some levels however the judges for the Formula Student seem to like it. Because of the shape of the bodywork, 2x200grm either side of 3mm Soric is pretty strong. Certainly strong enough for this application.

Warren

Carbon Copies Ltd
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I do find the use of jute and flax a bit of a false economy especially if your part needs some stiffness to it.  Both are very weak fabrics compared to carbons, so any environmental credentials are wiped out because you need to use more layers and as a consequence, more harmful resins to wet out the laminate.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
kekko81
kekko81
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 9, Visits: 50
very nice! great work
mhdghoul (01/02/2012)
hey people , please see the pics and hope u like it and if u liked it follow meSmile and if you need any help what so ever contact me.

wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Keep us posted then. I am currently working on a Formula Student car, and to gain some eco points we are using Jute and Flax for parts of the bodywork. It infuses well but does come out a bit of a poo brown colour Smile

Warren

Carbon Copies Ltd
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I'm involved with the whole project, including the chassis building and geometry design. I'm really looking forward to the body work though as part of the Eco theming we'll be using as much flax and jute as possible

It certainly does, when I started I was just doing little ducts and bits for cars, but I've since worked with a prosthetic part and tea trays, you never know what's coming.

The compos could definitely do with being carbon, they weigh a ton. The person who got me interested in composites and taught me the basics was a guy called Steve Thomas who worked for Dymag and did a lot with their motorbike wheels. I don't the the full process but he showed me the inflatable bladder he had for making the spoked section of the wheel.

We also have a Dymag rim which was part of a two piece wheel, the outer being carbon and the face being alloy