Finished the mould and pulled the first half of an oil catch tank for a customers Hillclimb car. The plan is to pull a second half, bond the two together and then trim off the flange. Done with infusion 200grm CF - 2 x 290grm E Glass - 200grm CF. Weight of one half is 123grms, could probably loose one layer of E Glass. Capacity when finished will be 2 ltrs.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
Replies
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
First 1L capacity Catch Tank finished.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
wozza (26/02/2014)
First 1L capacity Catch Tank finished.

Warren


Nice job, like the pushfittings to get the level indicator :-)
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Looks great! Did you use a gelcoat? I kind of see a blue-ish misty layer? or is it just the camera-flash?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
matthieutje65 (27/02/2014)
Looks great! Did you use a gelcoat? I kind of see a blue-ish misty layer? or is it just the camera-flash?


Hi Matthieu, bit of both I thinkSmile

I used GC50. With the mould being quite deep and narrow I may of laid it down a bit heavy with the gelcoat gun. I use GC50 often not just for UV protection but mainly in this case to act like spray tack to hold the first layer of cloth in place.

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wozza - 11 Years Ago
carbonfibreworks - 11 Years Ago
wozza - 11 Years Ago
carbonfibreworks - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
FLD - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
Djekouk - 11 Years Ago
matthieutje65 - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
wozza - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search