Finished the mould and pulled the first half of an oil catch tank for a customers Hillclimb car. The plan is to pull a second half, bond the two together and then trim off the flange. Done with infusion 200grm CF - 2 x 290grm E Glass - 200grm CF. Weight of one half is 123grms, could probably loose one layer of E Glass. Capacity when finished will be 2 ltrs.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Nice work Warren.

Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren

Carbon Copies Ltd
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
wozza (19/02/2014)
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren
Hi Warren
Almost done Smile working on some strange items at the moment plus preparing my race bike for the start of the season.
Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K

carbonfibreworks (19/02/2014)
wozza (19/02/2014)
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren
Hi Warren
Almost done Smile working on some strange items at the moment plus preparing my race bike for the start of the season.
Regards Chris


Sounds interestingSmile Look forward to seeing some pics of the Atom in all its glory. A lot of the work I am doing is covered by NDA's so can't post pics which is a bit frustratingCrying

Warren

Carbon Copies Ltd
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Is this a functioning oil/air separator or more of a flashy empty can? Ie. does it have any internal baffles to catch the oil? Not a dig, just wondering and interested to know how you put the baffles in place if it has them?

Also interested to know how you're attaching the fittings? 
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hanaldo (20/02/2014)
Is this a functioning oil/air separator or more of a flashy empty can? Ie. does it have any internal baffles to catch the oil? Not a dig, just wondering and interested to know how you put the baffles in place if it has them?

Also interested to know how you're attaching the fittings? 



Hi, its a flashy empty can Smile Because its a race engine and tends to "breath" a bit heavier than a standard engine the regulations require an "oil reservoir" to be fitted. He is using a plastic washer bottle at the momentSmile
Threaded inserts will be bonded on to take the hose tails and two push in air fittings and some PVC clear tube will be used as a level indicator.

Warren

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Beer can on my car BigGrin
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
FLD (20/02/2014)
Beer can on my car BigGrin



Red Bull cans seem popular also Smile

Carbon Copies Ltd
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
First 1L capacity Catch Tank finished.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search