Group: Forum Members
Posts: 688,
Visits: 5.4K
|
Finished the mould and pulled the first half of an oil catch tank for a customers Hillclimb car. The plan is to pull a second half, bond the two together and then trim off the flange. Done with infusion 200grm CF - 2 x 290grm E Glass - 200grm CF. Weight of one half is 123grms, could probably loose one layer of E Glass. Capacity when finished will be 2 ltrs.
Warren
Carbon Copies Ltd
|