Oil Catch Tank


Author
Message
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Finished the mould and pulled the first half of an oil catch tank for a customers Hillclimb car. The plan is to pull a second half, bond the two together and then trim off the flange. Done with infusion 200grm CF - 2 x 290grm E Glass - 200grm CF. Weight of one half is 123grms, could probably loose one layer of E Glass. Capacity when finished will be 2 ltrs.

Warren

Carbon Copies Ltd
Edited 11 Years Ago by wozza
Replies
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Nice work Warren.

Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren

Carbon Copies Ltd
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
wozza (19/02/2014)
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren
Hi Warren
Almost done Smile working on some strange items at the moment plus preparing my race bike for the start of the season.
Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K

carbonfibreworks (19/02/2014)
wozza (19/02/2014)
carbonfibreworks (19/02/2014)
Nice work Warren.

Chris


Cheers Chris, its only 220mm long and 110mm OD so was a bit of a pain to lay-up Doze
Hows the Atom project coming along?

Warren
Hi Warren
Almost done Smile working on some strange items at the moment plus preparing my race bike for the start of the season.
Regards Chris


Sounds interestingSmile Look forward to seeing some pics of the Atom in all its glory. A lot of the work I am doing is covered by NDA's so can't post pics which is a bit frustratingCrying

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wozza - 11 Years Ago
carbonfibreworks - 11 Years Ago
wozza - 11 Years Ago
carbonfibreworks - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
FLD - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
Djekouk - 11 Years Ago
matthieutje65 - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
wozza - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search