Bending cured pepreg


Author
Message
Steve Broad
Steve Broad
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
This may be of interest to someone :-)



Edited 6 Years Ago by Steve Broad
Replies
Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh I've done this before for patching holes in bodywork on panels with slight curvature. Just be aware that it does actually stress the carbon and make it quite weak.
Steve Broad
Steve Broad
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 6/8/2020 12:01:29 AM
Yeh I've done this before for patching holes in bodywork on panels with slight curvature. Just be aware that it does actually stress the carbon and make it quite weak.

I am surprised that it has that much of a weakening effect. However, this was going to be used to adjust a door shut line so that wouldn't be an issue.