Hello all, Im new to the forum and new to making composite parts. I have made a couple of splitter vents for a race car of mine and now am working on brake cooling ducts for the front air dam. 

My question is how to lay up the carbon fiber to ensure a reasonable release from the mold. It currently looks like this:




I was thinking I could lay it up (after sanding and smoothing of course), as is, vacuum bag it, and essentially make it as one piece. But as I read a couple of other posts on this forum I started to second guess myself. Any suggestions from the collective?

Thanks in advance!

  
Replies
AlpineCoupe
A
Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)Supreme Being (429 reputation)
Group: Forum Members
Posts: 45, Visits: 2.1K
Just wanted to say that I moved forward with primer and clear coat on this mold. Going to do some finish sanding and then seal the mold in some way. Thinking I might go with partall wax and PVA just took be sure I don't get any lock up. Can anyone confirm this to be a reasonable idea? If not, no offense taken I'd rather do it the right way! 


Edited 6 Years Ago by AlpineCoupe
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
AlpineCoupe - 11/4/2019 2:19:45 AM
Just wanted to say that I moved forward with primer and clear coat on this mold. Going to do some finish sanding and then seal the mold in some way. Thinking I might go with partall wax and PVA just took be sure I don't get any lock up. Can anyone confirm this to be a reasonable idea? If not, no offense taken I'd rather do it the right way! 


I usually just use a paste wax (formula five) for the plug and as i had good luck with partall in the past I'm sure this would work. However, as it is a brake duct and you probably don't have big requirements in the surface quality you could use some PVA on top of that. Belt and suspenders type approach.
I hate PVA and think it is too fiddly tho

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
Mikerw - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
             Thank you, that's very helpful!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
             Thanks! That's a good suggestion!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
AlpineCoupe - 5 Years Ago
AlpineCoupe - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search